This was another one of those massively wide-lipped platters. Because that rim is actually hollow, it is one of the lighter platters I made. Probably only 15" in diameter, it is a good five pounds lighter than a platter of a "normal" rim.
The inside of this platter was originally supposed to be bright fire-engine red...and crunchy! I think in my hurry to get things ready for this firing, I cut back on my thoroughness in the glaze lab, and didn't mix this glaze as thoroughly as was needed. My guess is that the lead frit in this glaze simple settled in the slurry.
In the end, it is certainly not what I expected, but it also has intriguing aspects. And it does really resemble dried up toothpaste, in bed.